Product details
Category: Strengthen porcelain>强化瓷土
Category:Strengthen porcelain
Model:D-69
Time:2017/12/6
Info:烧成温度:1270-1300
Parameter:
Category: Strengthen porcelain>强化瓷土
Category:Strengthen porcelain
Model:D-69
Time:2017/12/6
Info:烧成温度:1270-1300
Parameter: